FIELD: water purification. SUBSTANCE: coagulant is produced from nepheline-containing material treated with aqueous solution containing 1-170 g/l of free sulfuric or hydrochloric acid at temperature of 20-80 C and acid consumption equalling 50-85% of theoretically needed amount for reaction with acid-soluble components of initial material. Nepheline-containing material before acid treatment is ground to size of 120 mcm and smaller. When using pure solution of acid, solution contains 50-170 g/l of sulfuric or hydrochloric acid. Coagulant may also be prepared by treatment of nepheline with aqueous solution of aluminium of iron sulfate or chloride containing 1-100 g.l of free sulfuric or hydrochloric acid. Method allows production of complex reagent possessing coagulating, flocculating, turbidifying and neutralizing properties that increases its efficiency in water purification. EFFECT: higher efficiency. 4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING ALUMOSILICIC COAGULANT-FLOCCULANT | 2009 |
|
RU2421400C1 |
METHOD OF PRODUCING OF MIXED ALUMINIUM PHOSPHATES AND ALKALINE METALS | 1992 |
|
RU2022920C1 |
METHOD OF PREPARING COAGULATION-FLOCCULATION REAGENT AND WATER TREATMENT PROCESS | 1997 |
|
RU2131849C1 |
AVENTURINE GLASS | 1995 |
|
RU2100301C1 |
POTASSIUM ALUM PRODUCTION METHOD | 2007 |
|
RU2350564C2 |
METHOD OF PREPARING BADDELEYITE CONCENTRATE | 1998 |
|
RU2139250C1 |
BLACK GLASS | 1993 |
|
RU2049746C1 |
METHOD FOR PROCESSING DOLOMITE | 1996 |
|
RU2104935C1 |
METHOD OF PROCESSING OF SPHENE CONCENTRATE | 2000 |
|
RU2179528C1 |
METHOD OF PROCESSING OF LOPARITE CONCENTRATE | 2000 |
|
RU2182887C2 |
Authors
Dates
1995-07-20—Published
1992-02-25—Filed