FIELD: production of high-quality coke by slow coking.
SUBSTANCE: proposed method includes extraction of coal tar by mixture of aliphatic and aromatic solvents. Preliminarily, fraction is separated from coal tar at temperature of 80-230 C. Residue of coal tar boiling-off at temperature of 230 C is subjected to extraction. Used as mixture of aliphatic and aromatic solvents is mixture of white spirit and solvent boiling-off at temperature of 130-185 C at ratio of white spirit and solvent by mass of 2;1-3:1. Raffinate after distillation of said mixture of solvents, use if made of coal tar pitch at softening temperature of 85-95 C and distilled mixture of solvents is returned to extraction stage. Used as mixture of solvents is mixture of white spirit and solvent having density of 770-790 kg/cu m at temperature of 20 C and refraction index n
EFFECT: enhanced separation of solvent form extracting agent; reduced power requirements.
2 cl, 1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARING RAW MATERIAL FOR MAKING NEEDLE COKE | 0 |
|
SU1052163A3 |
LOW-TEMPERATURE CHEMICAL METHOD OF PRODUCING FULLERENE | 2011 |
|
RU2484011C2 |
METHOD OF PRODUCING HIGH-AROMATIC PITCH-LIKE PRODUCT | 0 |
|
SU1048988A3 |
METHOD OF SIMULTANEOUS PREPARING OF AROMATIC AND ALIPHATIC SOLVENTS | 1991 |
|
RU2024588C1 |
METHOD OF PRODUCING FULLERENE-POLYSULPHONIC ACID | 2011 |
|
RU2484012C1 |
METHOD FOR SEPARATING BYPRODUCTS AND WASTE IN METALLURGICAL INDUSTRY | 0 |
|
SU1801029A3 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2015 |
|
RU2586139C1 |
PROCESS FOR PRODUCING HYDROCARBON SOLVENTS | 0 |
|
SU1035053A1 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2014 |
|
RU2582411C1 |
COAL-TAR PITCH PROCESSING METHOD | 2004 |
|
RU2255956C1 |
Authors
Dates
2004-07-27—Published
2003-05-22—Filed