FIELD: corrosion protection.
SUBSTANCE: metal surface is treated with aqueous solution containing zinc, nitrate, nickel, and chlorate ions and, when fine-crystalline corrosion-resistant phosphate coating is to obtain at phosphatation temperature 30-45оС within a period of time 2 to 10 min, aqueous solution additionally contains calcium ions, concentrations of ions being the following, g/L: Zn2+ 1.527-3.225, P2O5 4.347-8.385, NO
EFFECT: reduced phosphatation temperature and time, lowered surface density of coating and consumption of phosphate concentrate, and avoided use of correcting solution.
3 ex
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF RECEIVING OF PHOSPHATE COATING | 2007 |
|
RU2354747C1 |
| PHOSPHATE COATING PRODUCTION METHOD | 2018 |
|
RU2690876C1 |
| METHOD OF MANUFACTURE OF PHOSPHATE COATING | 2007 |
|
RU2365675C2 |
| METHOD OF IRON-COBALT ALLOY PHOSPHATING | 2014 |
|
RU2560891C1 |
| SOLUTION FOR METAL SURFACE PHOSPHATIZING | 2001 |
|
RU2194800C2 |
| METHOD OF DEPOSITING PHOSPHATIZING COMPOSITION | 2002 |
|
RU2225895C2 |
| SOLUTION FOR PHOSPHATING | 1993 |
|
RU2065892C1 |
| PHOSPHATIZING SOLUTION | 0 |
|
SU1737020A1 |
| METHOD OF PHOSPHATIZING METALLIC SURFACE | 1996 |
|
RU2113541C1 |
| METHOD FOR PHOSPHATING METALLIC SURFACE | 2000 |
|
RU2210624C2 |
Authors
Dates
2004-11-20—Published
2002-08-05—Filed