FIELD: manufacture of building materials.
SUBSTANCE: carbonate-based raw mix contains 9.5-11.5% clay component, 1.8-2.0% iron-containing component, and 0.5-0.6% of neutralization sediment of effluent from chemical department of ferroalloy plant. The sediment is composed of, wt%: V2O5 3.58, MnO2 10.1, CaO 30, Fe2O3 0.62, MgO 1.03, TiO2 0.5, and Al2O3 0.12.
EFFECT: increased degree of decarbonization, reduced consumption, increased productivity of rotary oven, and improved grinding capability of clinker.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MATERIAL MIXTURE FOR OBTAINING PORTLAND-CEMENT CLINKER | 2008 |
|
RU2365549C1 |
RAW MIXTURE FOR PREPARING CEMENT CLINKER | 0 |
|
SU697426A1 |
RAW MIXTURE FOR PRODUCTION OF PORTLAND CEMENT CLINKER | 2002 |
|
RU2215703C1 |
RAW MIXTURE FOR PRODUCING PORTLAND CEMENT CLINKER | 0 |
|
SU1165659A1 |
RAW MIXTURE FOR PRODUCING PORTLAND CEMENT CLINKER | 0 |
|
SU1265168A1 |
FEEDSTOCK MIXTURE FOR PRODUCING CEMENT CLINKER | 1997 |
|
RU2101247C1 |
METHOD OF PRODUCING PORTLAND CEMENT | 2012 |
|
RU2509063C1 |
METHOD OF PRODUCING CEMENT ON BELITE CLINKER AND SLOW-CURING CEMENT OBTAINED ON ITS BASIS | 2020 |
|
RU2736594C1 |
RAW MIX FOR PREPARING PORTLAND CEMENT CLINKER | 0 |
|
SU1031933A1 |
RAW MATERIAL MIXTURE FOR PRODUCTION OF PORTLAND CEMENT CLINKER | 1996 |
|
RU2074135C1 |
Authors
Dates
2004-11-27—Published
2003-05-05—Filed