FIELD: medicine, oral surgery.
SUBSTANCE: composition of the suggested carboplastic contains a carbon tissue of TGN-2M type and polyamide film 12/10, additionally, it contains the powder of metallic boron. Components are taken at certain quantitative ratio. The suggested composition of carboplastic in question is of high physico-mechanical properties, constant roentgenocontrast. It is, also, nontoxic and not carcinogenic.
EFFECT: higher efficiency.
3 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION OF BLACK-REINFORCED PLASTIC FOR BONE DEFECT CORRECTION | 2007 |
|
RU2341294C1 |
COAL-PLASTIC COMPOSITION FOR BONE DEFECTS ELIMINATION | 2007 |
|
RU2342161C1 |
COAL-PLASTIC COMPOSITION FOR BONE DEFECTS ELIMINATION | 2007 |
|
RU2342160C1 |
COMPOSITION OF BLACK-REINFORCED PLASTIC FOR BONE DEFECT CORRECTION | 2007 |
|
RU2341295C1 |
COMPOSITION OF RADIOPAQUE PLASTIC FOR ELIMINATING BONE DEFECTS AND METHOD OF OBTAINING IT | 2020 |
|
RU2749024C1 |
CARBONPLASTIC ENDOPROSTHESIS FOR TEMPOROMANDIBULAR JOINT | 2015 |
|
RU2618948C2 |
CARBON-CARBON COMPOSITIONAL MATERIAL | 2008 |
|
RU2391118C1 |
METHOD FOR PRODUCTION OF LAMINATED PLASTIC | 2004 |
|
RU2271935C1 |
CARBON-CERAMIC FIBER-REINFORCED COMPOSITE MATERIAL AND METHOD FOR ITS OBTAINING | 2017 |
|
RU2684538C1 |
METHOD OF MAKING CARBON CERAMIC OBJECTS FROM CARBON CERAMIC MATERIAL | 2006 |
|
RU2345972C2 |
Authors
Dates
2004-12-10—Published
2003-11-27—Filed