FIELD: iron metallurgy, in particular steel treatment.
SUBSTANCE: claimed method includes crushing of burning components and blending with reflux agent (e.g. synthetic calcium fluoride). Oxides of doping elements used as oxidizing components are premixed with melted reflux agent preliminary with lower melting point than the same of steel, at volume ratio preferably 1:1-1:5, respectively, cooled, crushed in form of failing, and introduced to mixture of burning components and reflux agent.
EFFECT: method with improved fire- and explosion safety.
4 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
EXOTHERMIC SLAG FORMING MIXTURE | 0 |
|
SU1036434A1 |
EXOTHERMIC SLAG FORMING MIXTURE | 0 |
|
SU944754A1 |
EXPLOSIVE RETARDER | 2002 |
|
RU2235708C2 |
SLAG-PRODUCING MIXTURE FOR TREATMENT OF CAST IRON AND STEEL | 0 |
|
SU777069A1 |
ALUMINIUM POWDERED MATERIAL AND METHOD OF OBTAINING THEREOF | 2006 |
|
RU2344989C2 |
LIQUID STEEL HEATING METHOD | 2001 |
|
RU2195503C1 |
EXHOTHERMIC MIX FOR PRODUCING SLAG AND METAL MASTER ALLOY | 0 |
|
SU1100320A1 |
EXOTHERMAL MIXTURE FOR MELTING AND ALLOYING STEEL | 2000 |
|
RU2175017C1 |
METHOD OF FORMING WATER-FILLED EXPLOSIVE AND WATER-FILLED EXPLOSIVE CHARGE, WATER- FILLED EXPLOSIVE (OPTIONS) | 2001 |
|
RU2207331C2 |
EXOTHERMIC SLAG FORMING MIXTURE | 0 |
|
SU1006046A1 |
Authors
Dates
2005-01-20—Published
2003-08-07—Filed