FIELD: mining industry, particularly use of explosive substances based on calcium oxide for developing decorative rock, for safe breaking building structures and objects taken out of service.
SUBSTANCE: method involves reducing limestone to powder state, mixing powder with fine solid fuel; granulating thereof; high-temperature roasting the obtained granules in bed by penetration method under temperature of not less than 1500°C; grinding roasted granules to obtain the following fractional composition (% by weight): particles with 0.1 mm or lesser size- 30-50, particles with 0.1-0.25 mm size - 25-40, particles with 0.25-0.5 mm size - 15-25, particles with 0.5 mm and greater size - up to 20. To provide increased expansion clinker binding agent, for instance Portland cement taken in amount of 10-30% of roasted product mass is added to roasted granules.
EFFECT: improved quality, increased inner friction of hardening mix, provision of breaking force exceeding 180 MPa and 1.5-2 fold cost reduction in comparison with prior art method using rotary furnaces.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF NON-EXPLOSIVE DISINTEGRATOR BY SINTERING | 2013 |
|
RU2567254C2 |
METHOD FOR PREPARATION OF ANHYDRITE BINDER | 2007 |
|
RU2362748C1 |
EXPANSION ADDITIVE, HYDRAULIC BINDER WITH INDICATED ADDITIVE, AND A METHOD FOR PREPARATION THEREOF | 2002 |
|
RU2211194C1 |
METHOD OF PROCESSING MINERAL STOCK AND DEVICE TO THIS END (VERSIONS) | 2008 |
|
RU2402499C2 |
METHOD OF PRODUCING PORTLAND CEMENT | 2020 |
|
RU2742384C1 |
PRODUCTION OF HIGH-STRENGTH HIGH-EARLY-STRENGTH ALITE PORTLAND CEMENT AND PRODUCTION LINE TO THIS END | 2012 |
|
RU2520739C2 |
METHOD FOR PRODUCTION OF CEMENT CLINKER ON CONVEYOR GRATING | 1992 |
|
RU2049749C1 |
METHOD OF PRODUCTION OF LIME AND THE INSTALLATION FOR ITS REALIZATION | 2005 |
|
RU2287496C1 |
FIBROUS NANOCEMENT AND PREPARATION METHOD THEREOF | 2015 |
|
RU2595284C1 |
METHOD OF BAKING BINDING MATERIALS | 2007 |
|
RU2341476C1 |
Authors
Dates
2005-05-10—Published
2003-12-16—Filed