FIELD: refractory industry; manufacture of monolithic linings.
SUBSTANCE: proposed silicon-carbide concrete contains the following components, mass-%: plasticizing agent, 0.3-0.5; microsilica, 2.0-5.0; high-alumina cement, 7.0-10.0; the remainder being silicon carbide. Concrete may additionally contain high-alumina component at content of Al2O3 no less than 95 mass-% in the amount of 5-15 mass-%, for example in form of synthetic corundum of fraction lesser than 50 mcm or dust from electric filters of calcination furnaces in alumina production process.
EFFECT: enhanced strength of concrete at 600-1000°C; enhanced resistance to oxidation.
4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
CONCRETE MASS | 2011 |
|
RU2462435C1 |
FIREPROOF CEMENT-FREE CONCRETE MASS | 2013 |
|
RU2546692C2 |
RAW MATERIAL FOR HEAT-RESISTANT HEAT-INSULATING TORCRETE | 2018 |
|
RU2674484C1 |
RAW COMPOUND FOR FIREPROOF HEAT INSULATING CONCRETE | 2006 |
|
RU2329998C1 |
REFRACTORY CONCRETE MIX (VERSIONS) | 2003 |
|
RU2239612C1 |
REFRACTORY CONCRETE MIXTURE | 2018 |
|
RU2698390C1 |
FIRE-PROOF CONCRETE COMPOSITION | 2014 |
|
RU2550626C1 |
FIREPROOF CONCRETE MIX (VERSIONS) | 2011 |
|
RU2437862C1 |
MANUFACTURING METHOD OF CERAMIC PLATE BLOCKS FOR CREEP ANNEALING FURNACE | 2012 |
|
RU2485426C1 |
RAW MIX FOR PRODUCTION OF POROUS, FIREPROOF, HEAT INSULATION MATERIAL | 2008 |
|
RU2387623C2 |
Authors
Dates
2005-07-27—Published
2004-07-30—Filed