FIELD: road-transport industry.
SUBSTANCE: method includes applying substance on asphalt-concrete mixture. As substance silicon-organic modifier is used, loss of which at 1 m2 of area of pre-placed on road asphalt-concrete mixture at temperature 80-100°C is no less than 0,3-0,5 kg. After applying modifier, asphalt-concrete mixture is rolled.
EFFECT: higher efficiency, no corrosive effect on metals, effective at temperature above -20°C.
2 cl, 3 tbl, 3 ex, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARING ANTI-GLAZING REAGENT | 2002 |
|
RU2211235C1 |
ANTI-ICING COMPOSITION AND PREPARATION METHOD THEREOF | 2009 |
|
RU2408646C1 |
ANTI-ICING REAGENT AND METHOD FOR USE THEREOF | 2012 |
|
RU2500708C1 |
METHOD FOR TREATING ROAD COVERING | 2015 |
|
RU2674672C2 |
SOLID ANTIICING COMPOSITION AND A METHOD FOR REMOVING ICE FROM ROAD SURFACES | 2005 |
|
RU2294352C1 |
UNIVERSAL ANTI-ICING COMPOSITION | 2014 |
|
RU2564998C1 |
HARD ANTIICING COMPOSITION | 2000 |
|
RU2167179C1 |
COMPOSITION OF THE ANTI-ICING WATER SOLUTION FOR ROADS SURFACE TREATMENT | 2004 |
|
RU2264429C1 |
ANTI-GLAZE COMPOSITION | 2012 |
|
RU2521381C2 |
METHOD FOR MAKING ROAD CARPET | 2007 |
|
RU2374381C2 |
Authors
Dates
2005-09-10—Published
2003-07-14—Filed