FIELD: highway engineering, in particular paving upper layers building in all climatic regions.
SUBSTANCE: claimed bituminous concrete composition contains (mass %): lime chip of 5-20 mm fraction 35-45; petroleum viscous bitumen 5.0-5.5; mineral powder from dolomite or lime rocks 3-8; polymer additive 0.1-0.25 based on bitumen mass and balance: sand of 5 mm or less fraction. As said polymer additive polyethylene terephthalate in form of secondary plastic bottles is used.
EFFECT: bituminous concrete with improved structure-forming characteristics and increased water and heat resistance.
1 cl, 4 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
ASPHALT CONCRETE MIX | 2021 |
|
RU2777276C1 |
ASPHALT-CONCRETE MIXTURE | 2012 |
|
RU2487095C1 |
METHOD OF PRODUCING COLD ASPHALT CONCRETE MIXTURE BASED ON MODIFIED POLYMER-BITUMEN COMPOSITION | 2023 |
|
RU2824525C1 |
ASPHALTIC CONCRETE MIX | 2001 |
|
RU2204539C2 |
REPAIR MIXTURE FOR ASPHALT CONCRETE COVERINGS | 2022 |
|
RU2819692C2 |
ROAD CONCRETE MIX | 2008 |
|
RU2380331C1 |
ROAD MIX | 2011 |
|
RU2458092C1 |
RUBBERISED VIBRO CAST ASPHALT MIX | 2010 |
|
RU2435743C1 |
ASPHALT CONCRETE MIXTURE | 1997 |
|
RU2119465C1 |
ASPHALT-CONCRETE MIXTURE | 2011 |
|
RU2460703C1 |
Authors
Dates
2005-10-20—Published
2004-04-06—Filed