FIELD: metallurgy; by-product coke industry; production of coal-tar pitch used for preparation of graphitized products and anode mass.
SUBSTANCE: proposed method includes treatment of average-temperature pitch with air at elevated temperature at simultaneous delivery of air heated to temperature 120-250°C at rate of 1-10 m3/Tpitch at delivery of fraction of coal-tar resin in the amount of 5-30% of total amount of pitch.
EFFECT: improved quality of pitch due to reduced content of volatile matter and increased content of α-fraction.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING PITCH BINDER FOR ELECTRODE MATERIALS | 1996 |
|
RU2119522C1 |
METHOD OF PREPARING BINDING DITCH FOR ELECTRODE MATERIALS | 2002 |
|
RU2241016C2 |
METHOD OF PRODUCING HIGH-TEMPERATURE PITCH FOR PRODUCTION OF PITCH COKE | 1999 |
|
RU2176657C2 |
METHOD OF PREPARING BINDING PITCH FOR ELECTRODE MATERIALS | 2005 |
|
RU2288938C1 |
METHOD FOR PRODUCING COKE WITH A PSEUDOISOTROPIC MICROSTRUCTURE | 2020 |
|
RU2761201C1 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2015 |
|
RU2586139C1 |
RADIATION-THERMAL PRODUCTION OF BINDER-PITCH FOR FABRICATION OF ELECTRODES | 2014 |
|
RU2571152C2 |
METHOD OF PITCH PRODUCTION | 0 |
|
SU857224A1 |
METHOD FOR PREPARING ELECTRODE PITCH | 0 |
|
SU1097640A1 |
PROCESS FOR PRODUCING ELECTRODE PITCH | 0 |
|
SU1081196A1 |
Authors
Dates
2006-02-10—Published
2004-07-06—Filed