FIELD: electrode industry.
SUBSTANCE: coal pitch or its mixture with coal tar fractions, or with pitch distillates is treated with air within temperature range 35-380oC at air consumption below 10 m3/t.h and than subjected to heat aging at 350-380oC for 5 to 12 h.
EFFECT: enabled high-yield preparation of standard sorts of binding pitch with high content of α-fraction and reduced yield of volatiles from low-pyrolized coal tar.
3 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING BINDING PITCH FOR ELECTRODE MATERIALS | 2005 |
|
RU2288938C1 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2015 |
|
RU2586139C1 |
METHOD OF PRODUCING PETROLEUM-AND-CARBON COAL BINDER | 2019 |
|
RU2729803C1 |
RADIATION-THERMAL PRODUCTION OF BINDER-PITCH FOR FABRICATION OF ELECTRODES | 2014 |
|
RU2571152C2 |
METHOD OF PREPARING PITCH BINDER FOR ELECTRODE MATERIALS | 1996 |
|
RU2119522C1 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2014 |
|
RU2582411C1 |
METHOD OF PRODUCING MESOMORPHIC-PHASE CARBON POWDER | 2009 |
|
RU2443624C2 |
METHOD OF PRODUCTION OF PITCH | 2004 |
|
RU2269565C1 |
ANODIC MASS PRODUCTION METHOD | 2001 |
|
RU2196192C2 |
METHOD OF PRODUCING MODIFIED BINDERS AND IMPREGNATING PITCHES | 2023 |
|
RU2824121C1 |
Authors
Dates
2004-11-27—Published
2002-11-28—Filed