FIELD: manufacture of building materials.
SUBSTANCE: building mortar including Portland cement, sand, foaming agent, and water contains, as foaming agent, protein-containing substance modified with complex modifier M-3 consisting of 0.04% aqueous emulsion of colophony and 0.1% aqueous solution of gelatin using following proportions: 3.6-3.8% of protein-containing substance, 57.6-57.8% of colophony emulsion, and 38.5-38.6% of gelatin solution. Mortar further contains stabilizer, in particular orthosilicic acid (H4SiO4) sol with pH 3.1-4.0 and potassium ferricyanide additive. Total composition of mortar is thus as follows, wt %: Portland cement 40.770-42.410, sand 39.621-40.728, modified protein-containing foaming agent 2.311-2.374, orthosilicic acid sol 0.023-0.025, potassium ferrocyanide 0.061-0.063, and water 15.575-16.040. Mortar is suitable for use when mason's and plastering operations are carried out.
EFFECT: reduced mean density of mortar and heat conductivity coefficient, increased mortar stability.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
STEAM CURED FOAMED CONCRETE | 2004 |
|
RU2255074C1 |
BUILDING MORTAR | 2005 |
|
RU2283819C1 |
FOAMED CONCRETE MIX | 2006 |
|
RU2306300C1 |
FINISHING COMPOSITION | 2009 |
|
RU2402508C1 |
RAW MIX | 2004 |
|
RU2270818C1 |
RAW MATERIAL MIXTURE | 2005 |
|
RU2278840C1 |
RAW MATERIAL MIX FOR AUTOCLAVE FOAM CONCRETE | 2007 |
|
RU2354630C1 |
RAW MIXTURE | 2005 |
|
RU2278084C1 |
MIX FOR FOAM CONCRETE | 2006 |
|
RU2305087C1 |
RAW MATERIAL MIXTURE | 2009 |
|
RU2396235C1 |
Authors
Dates
2006-02-27—Published
2004-08-30—Filed