FIELD: construction.
SUBSTANCE: raw material mix for autoclave foam concrete includes, wt %: concrete 48.54-49.60, sand 5.82-6.23, protein-containing foaming additive Addimen Sb-31 0.34-0.36, fine-ground ash and slag waste of solid fuel combustion, with specific surface Ssp not less than 300 m2/kg 14.90-15.10, NaF additive 0.21-0.24, water 29.13-29.53.
EFFECT: enhanced compression durability, reduced heat conductivity rate, increased steam permeability rate.
2 ex, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIX FOR CELLULAR CONCRETE FABRICATION | 2009 |
|
RU2392252C1 |
MIX FOR FOAM CONCRETE | 2006 |
|
RU2305087C1 |
FOAMED CONCRETE MIX | 2006 |
|
RU2306300C1 |
STEAM CURED FOAMED CONCRETE | 2004 |
|
RU2255074C1 |
AUTOCLAVE FOAM-ASH CONCRETE | 2009 |
|
RU2395478C1 |
MIXTURE FOR AUTOCLAVE FOAM CONCRETE | 2011 |
|
RU2484066C1 |
AUTOCLAVE ASH FOAMED CONCRETE | 2004 |
|
RU2256632C1 |
MIXTURE FOR AUTOCLAVE FOAM CONCRETE | 2016 |
|
RU2624942C1 |
INSULATING CONCRETE | 2005 |
|
RU2278848C1 |
AUTOCLAVE ASH FOAM CONCRETE | 2017 |
|
RU2647712C1 |
Authors
Dates
2009-05-10—Published
2007-11-30—Filed