FIELD: metallurgy, possibly processes for making metallurgical semicoke.
SUBSTANCE: method comprises steps of heat treatment of coal layer in vertical shaft type apparatus while igniting at side opposite to that of air supply; using as raw material coal fractions 20 - 70 mm; supplying air through coal layer at specific flow rate 70 - 99.5 m3/m 2h depending upon coal kind.
EFFECT: possibility for obtaining solid product of higher strength, with lowered ash content and larger mean size of lumps at increased yield.
1 cl, 3 ex, 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METALLURGICAL MEDIUM-TEMPERATURE COKE PRODUCTION PROCESS | 2005 |
|
RU2288937C1 |
| METHOD OF PREPARING SEMICOKE | 2000 |
|
RU2169166C1 |
| METHOD OF THERMAL COAL ENRICHMENT | 2015 |
|
RU2637551C2 |
| METHOD FOR PRODUCING CARBON ADSORBENT | 1993 |
|
RU2014883C1 |
| METHOD FOR MAKING GAS CARBON AND SYNTHESIS GAS IN COAL CONVERSION | 2007 |
|
RU2345116C1 |
| METHOD OF PROCESSING CARBON-CONTAINING MATERIALS | 2023 |
|
RU2818245C1 |
| METHOD OF THE LAYERWISE COAL GASIFICATION | 2005 |
|
RU2287011C1 |
| METHOD OF PRODUCTION OF SEMI-COKE AND THE DEVICE FOR ITS REALIZATION | 2004 |
|
RU2278817C1 |
| METHOD OF COAL CONVERSION | 2009 |
|
RU2401295C1 |
| COAL PROCESSING METHOD | 2018 |
|
RU2722557C2 |
Authors
Dates
2006-04-27—Published
2004-12-03—Filed