FIELD: polymer materials.
SUBSTANCE: polymeric pressed composition is fabricated by impregnating basalt thread with liquid mixture of phenol and formaldehyde monomers in presence of sodium hydroxide catalyst at ratio 1:1.4:0.02, respectively, followed by polycondensation of resol phenol-formaldehyde oligomer at 90°C for 60 min at basalt thread-to-oligomer weight ratio 1:1, after which resulting material is dried for 15 min at 120°C and pressed for 9 min at 150°C and pressure 25 MPa to produce composite.
EFFECT: improved physico-mechanical properties of composites, which can be used in construction, instrumentation and mechanical engineering.
2 cl, 1 tbl, 13 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING OF POLYMERIC PRESS-COMPOSITION | 1991 |
|
RU2021301C1 |
METHOD OF PRODUCING POLYMERIC PRESS-COMPOSITION | 0 |
|
SU787434A1 |
METHOD OF MANUFACTURING PAPER MATERIAL FOR INTERNAL LAYER OF DECORATIVE PAPER-LAYERED PLASTIC | 1996 |
|
RU2096549C1 |
POLYMER BINDER FOR COMPOSITE REINFORCEMENT | 2010 |
|
RU2495892C2 |
POLYMER FRICTION COMPOSITION (VARIANTS) | 1993 |
|
RU2090578C1 |
METHOD OF PRODUCING PAPER FOR INNER LAYERS OF DECORATIVE LAMINATED PAPER PLASTIC | 0 |
|
SU1756445A1 |
0 |
|
SU1564166A1 | |
METHOD OF PREPARING POLYMERIC MOLDED MATERIAL | 1995 |
|
RU2128195C1 |
FRICTIONAL POLYMERIC COMPOSITION | 2004 |
|
RU2275394C2 |
METHOD OF REDUCING FORMALDEHYDE EMISSION FROM MINERAL FIBROUS ARTICLE AND MINERAL FIBROUS ARTICLE WITH REDUCED EMISSION OF FORMALDEHYDE | 2011 |
|
RU2591951C2 |
Authors
Dates
2006-05-20—Published
2004-12-08—Filed