FIELD: application of metallic coatings, possibly chemical deposition of composition type copper coatings onto steel parts that may be used in electric, chemical industry branches, in machine engineering.
SUBSTANCE: solution contains copper sulfate, sodium potassium tartrate, sodium sulfate, sodium hydroxide, Formalin, Aerosil and 20% aqueous solution of polyacrylamide at next relation of ingredients (g/l): copper sulfate, 4 - 5; sodium potassium tartrate, 20 - 22; sodium sulfate, 15 - 16; sodium hydroxide, 10 - 12; Formalin, 20 -24; Aerosil, 0.2 - 0.3; 20% aqueous solution of polyacrylamide, 0.5 - 3.
EFFECT: improved wear resistance, corrosion resistance in sea atmosphere due to increased thickness of coating, lowered friction factor.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
SOLUTION FOR MAKING COPPER POLYMER COATS | 2004 |
|
RU2263158C1 |
AQUEOS SOLUTION FOR CHEMICAL COPPER PLATING | 0 |
|
SU983149A1 |
PROCESS OF PRODUCTION OF SUPERCONDUCTOR CERAMIC COATINGS OF THE CUPRATE TYPE WITH THE PEROWSKITE STRUCTURE | 0 |
|
SU1830396A1 |
CHEMICAL COPPER PLATING SOLUTION | 0 |
|
SU1312119A1 |
AQUEOUS SOLUTION FOR CHEMICAL COPPER PLATING | 0 |
|
SU1138433A1 |
SOLUTION FOR CHEMICAL COPPERING | 2003 |
|
RU2238347C1 |
ELECTROLYTE FOR COPPER PLATING | 0 |
|
SU1761820A1 |
0 |
|
SU497359A1 | |
0 |
|
SU259591A1 | |
CHEMICAL COPPER PLATING SOLUTION | 0 |
|
SU1087565A1 |
Authors
Dates
2006-09-20—Published
2005-07-18—Filed