FIELD: textile industry.
SUBSTANCE: invention relates to finishing textile materials and can be used when manufacturing materials for technical articles, including defending hoods, awnings, individual layers of layered composite materials. Treatment process consists in impregnation of textile material first with 15-20% solution of 4,4'-diphenylmethanediisocyanate ε-caprolactam in organic solvent and then with 5-10% aqueous solution of phosphorus-boron-containing polyol having following formula: , where R represents -CH2-CH2-, p=1, q=3, and m=2. Each impregnation is followed by drying. As organic solvent, toluene, hexane, and benzene are used.
EFFECT: improved complex of performance characteristics due to imparting fireproofness and resistance to wet treatments to textile materials preserving their high physicochemical properties.
2 cl, 1 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
SIMULATED LEATHER | 2006 |
|
RU2307208C1 |
METHOD OF DECORATING TEXTILE MATERIALS | 0 |
|
SU855100A1 |
ARTIFICIAL SKIN | 1998 |
|
RU2142030C1 |
METHOD OF FINISHING TEXTILE MATERIALS | 0 |
|
SU883214A1 |
METHOD OF TREATING TEXTILE MATERIAL | 1994 |
|
RU2078865C1 |
ARTIFICIAL LEATHER | 1998 |
|
RU2134737C1 |
METHOD OF FINISHING TEXTILES | 0 |
|
SU836258A1 |
POLYURETHANE COATING COMPOSITION | 2008 |
|
RU2391362C2 |
METHOD FOR PREPARING PHOSPHORUS-BORON-CONTAINING POLYURETHANS | 2004 |
|
RU2275388C2 |
ARTIFICIAL LEATHER AND METHOD FOR PRODUCTION THEREOF | 1992 |
|
RU2010899C1 |
Authors
Dates
2007-09-27—Published
2006-05-26—Filed