FIELD: construction engineering; methods of restoration and application of protective coats on concrete surfaces.
SUBSTANCE: proposed method includes layer-by-layer application of binding primer layer and main concrete layer; prior to applying the binding primer layer, concrete or reinforced concrete surface is impregnated with 1- 10-% aqueous solution of hardening agent at flow rate of no less than 300 g/m2 and is held for at least 0.5 hour; used as binder of priming layer is composition containing Portland cement, micro-silica, superplasticizing agent C-3, organo-silicon fluid or aqueous emulsion of ornago-silicon fluid. This composition is applied at thickness of 1.5-3.0 mm and is held for 5-30 minutes after which main concrete layer, no less than 10 mm thick is applied.
EFFECT: enhanced durability and waterproofness of protective layer applied on horizontal and vertical surfaces; enhanced strength and freeze resistance.
5 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
WATER-TIGHTNESS RECOVERY METHOD FOR WATERPROOFING BUILDING STRUCTURE COATING | 2005 |
|
RU2287046C2 |
THERMOELECTRIC MAT | 2006 |
|
RU2320830C2 |
METHOD OF ELECTRICAL CURING OF CONCRETE IN WINTER | 2003 |
|
RU2250206C1 |
METHOD TO RECOVER WATER PERMEABILITY AND WATERPROOF COATING OF BUILDING STRUCTURES | 2005 |
|
RU2283405C1 |
BUILDING STRUCTURE WATER-TIGHTNESS AND WATERPROOF COVERING RECOVERY METHOD | 2004 |
|
RU2282007C1 |
THERMOELECTRIC MAT | 2005 |
|
RU2289891C1 |
METHOD TO PREVENT PEELING OF ROOF MADE OF BITUMEN ROLL MATERIAL | 2005 |
|
RU2299297C1 |
METHOD TO RECOVER WATER-TIGHTNESS OF BUILDING STRUCTURE WATERPROOFING COVERING | 2005 |
|
RU2304677C2 |
CORROSION MODIFYING AGENT | 2005 |
|
RU2291173C1 |
METHOD TO RECOVER WATER-TIGHTNESS OF WATERPROOFING BUILDING STRUCTURE COVERINGS | 2005 |
|
RU2293163C1 |
Authors
Dates
2007-10-10—Published
2006-02-06—Filed