FIELD: metallurgy.
SUBSTANCE: method comprises step of feeding onto metal heel in steel casting ladle heat insulation mixture containing, vol.%: expanded vermiculite or expanded pearlite with fraction size 0.6 - 2.5 mm, 60 - 70; wood saw-dust with fraction size 0.5 -5.0 mm, 30 -40. Heat insulation mixture is fed in polypropylene container. Bottom of such container is melt by action of metal temperature 1550-1600°C and mixture is distributed onto metal surface. Ladle is covered with lid for protecting metal and heat insulation mixture against oxygen access. Wooden dust is decomposed in atmosphere with oxygen deficiency for forming sooty carbon. Heat insulation powder is formed on metal surface containing nucleuses of expanded vermiculite or expanded pearlite covered with envelopes of sooty carbon. Such powder features high heat insulation properties.
EFFECT: lowered heat losses at soaking metal in steel casting ladle, elimination of "cold metal" on bottom of ladle and in steel casting nozzle.
5 cl, 2 dwg, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR HEAT INSULATION OF LIQUID METAL SURFACE | 2009 |
|
RU2405654C1 |
HEAT INSULATING AND PROTECTIVE MIXTURE FOR METAL SURFACE IN INTERMEDIATE LADLE OF CONTINUOUS-CASTING MACHINE | 2007 |
|
RU2334587C1 |
HEAT INSULATION MIXTURE | 0 |
|
SU602298A1 |
EXOTHERMIC SLAG FORMING MIXTURE FOR POURING STEEL | 0 |
|
SU1031638A1 |
HEAT INSULATION MIXTURE FOR CONTINUOUS CASTING OF METALS | 0 |
|
SU789219A1 |
MIXTURE FOR HEAT INSULATION OF METAL SURFACE AT STEEL CASTING | 0 |
|
SU833367A1 |
0 |
|
SU589067A1 | |
HEAT-INSULATING MIXTURE | 1994 |
|
RU2081720C1 |
HEAT INSULATION MIXTURE | 2005 |
|
RU2289493C1 |
METHOD OF THERMO INSULATION AND PROTECTION OF METAL SURFACE FROM OXIDATION IN INTERMEDIATE LADLE OF CONTINUOUS-CASTING MACHINE | 2007 |
|
RU2334586C1 |
Authors
Dates
2007-10-20—Published
2005-08-29—Filed