FIELD: metallurgy.
SUBSTANCE: mixture contains expanded vermiculite, saw dust, refractory powder and surface active substance at the following component ratio, wt %: expanded vermiculite 60-65, saw dust 29.9-37.7, refractory powder 2-5, surface active substance 0.1-0.3. Mixture has bulk density of 150 to 350 kg/m3.
EFFECT: providing heat-insulating effect till metal pouring is completed, and maintaining reference height of mixture layer.
6 cl
Title | Year | Author | Number |
---|---|---|---|
LIQUID METAL HEAT INSULATION METHOD | 2005 |
|
RU2308352C2 |
EXOTHERMIC MIXTURE FOR HEAT INSULATION OF THE HEAD PART OF THE INGOT DURING CASTING OF STEELS AND ALLOYS | 2022 |
|
RU2773977C1 |
HEAT INSULATION MIXTURE | 2005 |
|
RU2289493C1 |
HEAT INSULATING MIXTURE | 2008 |
|
RU2370340C1 |
EXOTHERMIC MIXTURE FOR HEATING OF INGOT HEAD PART DURING POURING OF STEELS AND ALLOYS | 2005 |
|
RU2284876C1 |
EXOTHERMIC SLAG FORMING MIXTURE FOR POURING STEEL | 0 |
|
SU1031638A1 |
COMPOSITION OF SLAG-MAKING BRIQUETTE FOR STEEL LADLE-TO-MOLD CASTING | 2003 |
|
RU2243270C1 |
HEAT-INSULATING MIXTURE | 2008 |
|
RU2384386C1 |
HEAT INSULATING MIXTURE | 2008 |
|
RU2369463C1 |
HEAT INSULATED INSERT FOR LINING OF HOT TOP OF INGOT MOLD | 2000 |
|
RU2176172C1 |
Authors
Dates
2010-12-10—Published
2009-11-05—Filed