FIELD: chemical and paint-and-varnish industries; production of inorganic pigments.
SUBSTANCE: proposed method includes leaching-out of serpentine ore mixture containing magnesium and chromium by sulfuric or hydrochloric acid for obtaining iron-containing solution which is treated with hydrogen peroxide and is neutralized to pH= 7.0-8.0. Suspension thus obtained is filtered and iron hydroxide residue is dissolved with sulfuric or hydrochloric acid, then it is treated with alkaline reagent to pH=2.0-6.0 and is filtered. Then, iron hydroxide residue is washed off water-soluble ions, dried and burnt at temperature of 550-700C.
EFFECT: wide range of tints in processing and decontamination of sulfate and chloride waste obtained at production of periclase and chromite concentrate.
2 cl, 5 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF INTEGRATED PROCESSING OF MAGNESIUM-CHROME CRUDE ORE | 2006 |
|
RU2344076C2 |
METHOD OF PRODUCTION OF CHROMITE CONCENTRATE | 2006 |
|
RU2312912C2 |
METHOD OF COMPLEX PROCESSING OF SERPENTINE-CHROMITE CRUDE ORE | 2013 |
|
RU2535254C1 |
MAGNESIUM OXIDE PRODUCTION PROCESS | 2004 |
|
RU2279404C1 |
METHOD OF COMPLEX TREATMENT OF SERPENTINITE | 2020 |
|
RU2739046C1 |
PROCEDURE FOR COMPLEX PROCESSING NICKEL-COBALT RAW MATERIAL | 2009 |
|
RU2393251C1 |
METHOD FOR INTEGRATED TREATMENT OF MANGANESE CARBONATE-OXIDE ORE | 2013 |
|
RU2539885C1 |
METHOD OF PROCESSING MAGNESIUM-CONTAINING MATERIALS | 2007 |
|
RU2369559C2 |
METHOD FOR PRODUCING MAGNESIUM SULPHATE AND IRON-OXIDE PIGMENTS FROM PRODUCTION WASTES | 2016 |
|
RU2634017C2 |
METHOD OF MANGANESE ORE PROCESSING | 2013 |
|
RU2539813C1 |
Authors
Dates
2007-11-10—Published
2006-02-08—Filed