FIELD: technological processes.
SUBSTANCE: method includes the following: viscose or polyacrylonitrile technical thread is soaked with the mixture of epoxy resin ED-20 and hardener polyethylene polyamine with mass ratio 9:1. Then bundle is formed out of separately soaked technical threads with the number of threads of 100-140 and is thermally treated at the temperature of 30-70°C. At the same time the shaped bundle is exposed to ultraviolet radiation with power of 0.70-0.80 Watt/m3 at the wave length of λ=253.7 for 8-12 minutes, and then hardened.
EFFECT: increases breaking stress during static bending of materials with polyacrylonitrile technical thread.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING REINFORCED POLYMER COMPOSITE MATERIALS | 1994 |
|
RU2102407C1 |
METHOD OF PREPARING REINFORCED POLYMERIC MATERIALS | 1997 |
|
RU2135530C1 |
METHOD OF FABRICATING REINFORCED POLYMER MATERIALS | 1996 |
|
RU2132341C1 |
METHOD FOR PRODUCTION OF REINFORCED POLYMER COMPOSITE MATERIALS | 2005 |
|
RU2280655C1 |
METHOD OF PRODUCING POLYMER ELECTRET | 2018 |
|
RU2696623C1 |
METHOD OF PRODUCING REINFORCED POLYMER COMPOSITE MATERIAL | 2013 |
|
RU2538271C1 |
METHOD OF OXIDATIVE STABILIZATION OF MOLDED POLYACRYLONITRIL PRODUCTS IN CARBON MATERIAL PRODUCTION | 0 |
|
SU1737037A1 |
UV TREATMENT OF COLEOPTERA LARVAE PROCESSED FOR VITAMIN D3 ENRICHMENT | 2020 |
|
RU2804480C1 |
METHOD OF PRODUCING FILTERING-SORBING MATERIAL WITH PHOTO CATALYTIC PROPERTIES | 2011 |
|
RU2482912C1 |
METHOD FOR PRODUCTION OF PREPREG | 1991 |
|
RU2028322C1 |
Authors
Dates
2008-05-20—Published
2007-03-15—Filed