FIELD: technological processes; measurement.
SUBSTANCE: method includes preparation of cement stone by means of its shredding. Cement stone immersion in corrosive solution is done in particles with size of 0.1 - 1.0 mm. Corrosive solution is selected from neutral or low alkaline medium in the form of sodium sulphide water solution. Cement stone soaking in corrosive solution is performed with continuous stirring with periodical sampling of liquid phase for chemical analysis for ion content. Determination of corrosion extent is done by change of sulphide-ions concentration. Method is characterised with reduction of corrosion detection time.
EFFECT: receipt of accelerated method for cement stone corrosion detection.
6 cl
Title | Year | Author | Number |
---|---|---|---|
GROUTING COMPOSITION | 2005 |
|
RU2305695C2 |
METHOD OF CONTROLLING DEVELOPMENT OF NONUNIFORM OIL FORMATION | 2005 |
|
RU2304706C2 |
ACID SURFACTANT COMPOSITION FOR TREATING HOLE-BOTTOM ZONE | 2005 |
|
RU2307149C2 |
METHOD TO PREVENT SALT DEPOSIT IN OIL- AND GAS-FIELD EQUIPMENT | 2005 |
|
RU2320852C2 |
TECHNOLOGICAL LIQUID FOR PERFORATION AND DAMPING HOLES | 2005 |
|
RU2309176C2 |
SOLUTION FOR CORROSION TESTS OF COPPER ALLOYS FOR TENDENCY TO SELECTIVE CORROSION | 0 |
|
SU1538101A1 |
METHOD FOR TECHNICAL CONTROL OF WELL SUPPORT CONDITION IN PROCESS OF ITS OPERATION | 2002 |
|
RU2249095C2 |
METHOD FOR PRESERVATION OF BOILER EQUIPMENT | 2021 |
|
RU2763083C1 |
METHOD FOR DETERMINING SEDIMENT COMPOSITION IN OIL PREPARATION EQUIPMENT | 2020 |
|
RU2743783C1 |
METHOD OF LEACHING AND EXTRACTION OF GOLD AND SILVER FROM PYRITE CINDER | 2019 |
|
RU2721731C1 |
Authors
Dates
2008-06-20—Published
2006-05-04—Filed