FIELD: mining.
SUBSTANCE: invention concerns mineral dressing, particularly flotation dressing methods, and can be applied in processing diamond-bearing ores. The method of diamond-bearing ore flotation involves non-polar black oil based collector, heteropolar collector, and foaming agent. Non-polar black-oil based collector is a black oil fraction obtained in the process of direct oil refining at 280°C and processed previously with MPK-3 depressor additive at the following component ratio: black oil fraction 99.6%, MPK-3 depressor additive 0.4%.
EFFECT: increased rate of diamond extraction to concentrate; improved process selectivity.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
USE OF OXYETHYLATED DERIVATIVES OF CASHEW NUTSHELLS LIQUID AS REAGENT-FOAMING AGENT FOR BENEFICIATION OF DIAMOND-CONTAINING ORES | 2019 |
|
RU2718880C1 |
METHOD OF FLOTATION SEPARATION OF SULPHIDES COMPRISING NOBLE METALS FROM COMPLEX IRON-CONTAINING ORE AND COMPOSITE MATERIAL TO THIS END | 2008 |
|
RU2393925C1 |
METHOD FOR BULK FLOTATION OF POLYMETALLIC ORES BASED ON USE OF MICROEMULSIONS | 2023 |
|
RU2821082C1 |
METHOD OF COAL FLOTATION AND COMPOSITE REAGENT TO THIS EFFECT | 2006 |
|
RU2333800C1 |
METHOD OF FROTH SEPARATION AND FLOTATION | 1989 |
|
RU1739566C |
METHOD OF COAL FLOTATION | 2016 |
|
RU2643873C1 |
COMPOSITION OF REAGENTS FOR FLOTATION ENRICHMENT OF GOLD-CONTAINING SULFIDE ORE | 2023 |
|
RU2810376C1 |
COMPOSITE REAGENT FOR COAL FLOTATION | 2016 |
|
RU2641626C1 |
METHOD OF FOAM SEPARATION AND FLOATATION | 1993 |
|
RU2065778C1 |
METHOD FOR FLOTATION ENRICHMENT OF SYLVINITE ORES | 2020 |
|
RU2776172C1 |
Authors
Dates
2008-09-20—Published
2006-06-19—Filed