FIELD: weapon and ammunition.
SUBSTANCE: method includes preparation of bore surface and coating. Bore surface is prepared with mixed native minerals and biological enzyme systems dissolved and suspended in isopropyl alcohol at temperature 50°...80°C within 60...90 minutes. Then it is covered with polyfunctioning composition of mixed homogeneous and heterogeneous catalysts and dispersion-hardening systems in viscous carrier. Further layer is heat-treated within 2...4 hours at temperature 110°...120°C. Then bore is assembled, firearm is loaded with bullet or shell and shooting is made for hardening of applied coating. Number of shots depends on barrel bore calibre.
EFFECT: provided antifriction, wear-resistant and anticorrosive protective coating of barrel bore; correction of its internal geometry and elimination of erosion-and-corrosion wear and internal splits.
2 cl, 4 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD TO FORM COATING OF INTERNAL SURFACE OF FIREARMS BARREL | 2011 |
|
RU2479672C1 |
METHOD OF PRODUCTION OF GUN BARREL | 2013 |
|
RU2557892C2 |
METHOD OF MAKING BORE WITH GROOVES | 2007 |
|
RU2353461C2 |
METHOD FOR MANUFACTURE OF FIREARM WEAR-RESISTANT BARREL | 1999 |
|
RU2169328C1 |
METHOD OF SMALL ARMS BARREL HARDENING | 2012 |
|
RU2499968C1 |
CARTRIDGE | 2002 |
|
RU2224208C2 |
METHOD FOR FORMING A PROTECTIVE COATING OF GUN BARRELS | 2021 |
|
RU2769032C1 |
METHOD TO APPLY MARKING SYSTEM ON INNER SURFACE OF GUN BARREL | 2009 |
|
RU2434195C2 |
DEVICE FOR APPLICATION OF TRIBOCOMPOSITION OF ARTILLERY SHELL | 2011 |
|
RU2572473C2 |
COMPOSITION FOR CLEANING GUN BARRELS | 2009 |
|
RU2391447C1 |
Authors
Dates
2008-11-20—Published
2007-01-25—Filed