FIELD: metallurgy.
SUBSTANCE: method includes hot rolling by two stages with accumulated closing 60-77% of breakdown bar cross-section area at each stage with soaking 19-26 s after the first and 12-17 s after the second with precooling of breakdown bar till temperatures not less then Ar3, definitive rolling in this range of temperatures, cyclic cooling of surface with quantity of cycles, equal to two, during time (0.017-0.020)D s in the first cycle and (0.05-0.06)D s in the second cycle with intermediary warm during 0.2-0.3 s and definitive warm of surface till temperatures which are lower then point Ac1 and definitive air cooling, where D - rolled iron diameter in mm.
EFFECT: increasing of plastic characteristics of fittings at saving of its strength characteristics.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
THERMOMECHANICAL TREATMENT METHOD FOR ROLLED METAL | 2011 |
|
RU2448167C1 |
PROCEDURE FOR FABRICATION OF ROD OF SCREW PROFILE | 2010 |
|
RU2425897C1 |
METHOD OF MAKING HIGH-STRENGTH HEAT-HARDENED REINFORCING-BAR STEEL | 2004 |
|
RU2287021C2 |
METHOD OF THERMOMECHANICAL TREATMENT OF ROLLED PRODUCTS | 1999 |
|
RU2169198C2 |
PROCEDURE FOR FABRICATION OF DOUBLE TEE FOR MINE MONO-RAIL WAYS | 2010 |
|
RU2425896C1 |
METHOD OF PRODUCING HEAT-HARDENABLE REINFORCING ROD STEEL | 1999 |
|
RU2149193C1 |
METHOD OF HEAT TREATMENT OF ROLLED STOCK | 2002 |
|
RU2227811C1 |
METHOD OF DEFORMATION-THERMAL PROCESSING LOW-ALLOY STEEL | 2016 |
|
RU2631068C1 |
METHOD OF HEAT TREATMENT OF ROLLED PRODUCTS | 1995 |
|
RU2081189C1 |
PROCEDURE FOR MANUFACTURE OF SPECIAL INTERCHANGEABLE PROFILE | 2010 |
|
RU2431688C1 |
Authors
Dates
2008-12-10—Published
2006-09-18—Filed