FIELD: chemistry, construction.
SUBSTANCE: binding agent includes, wt %: semi-water gypsum of β-modification -57.3-62.9, grinded basic granular blast-furnace slag - 15.2-16.25, caustic magnesite - 10.8-16.25, clyite dust from cyclones - 0.45-0.9, bischofite solution with density 1.2 g/cm3 in terms of magnesium chloride MgCl2 -9.75-10.2. Method of preparation of said binding agent includes mixing said gypsum, said slag and caustic magnesite, tempering of dry mixture with bischofite solution with density 1.2 g/cm3 and further introduction of said dust 1-2 min before formation.
EFFECT: increase of strength under compression, extension of stiffening terms, reduction of binding agent water resistance.
2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF GYPSUM-CONCRETE MIX PRODUCTION | 2007 |
|
RU2341481C1 |
BINDER | 2013 |
|
RU2532437C1 |
MOLDING BINDING MIXTURE | 1996 |
|
RU2118624C1 |
RAW MIX | 1998 |
|
RU2130437C1 |
METHOD OF MANUFACTURING GYPSUM-CONCRETE PRODUCTS | 0 |
|
SU1747420A1 |
METHOD OF MANUFACTURING PRODUCTS | 1995 |
|
RU2096380C1 |
METHOD OF PREPARING MOLDED RAW MATERIALS MIXTURE | 1991 |
|
RU2013408C1 |
RAW MIX | 2007 |
|
RU2363675C1 |
RAW FORMING MIXTURE | 1997 |
|
RU2114087C1 |
SELF-LEVELING CONSTRUCTION MIX FOR THE MANUFACTURE OF CONTINUOUS-POUR FLOORS | 2020 |
|
RU2763486C1 |
Authors
Dates
2008-12-20—Published
2007-03-30—Filed