FIELD: metallurgy.
SUBSTANCE: charge contains pig, recycled material, broken pieces, ferroalloys, limestone and coke, barium carbonate and strontium carbonate or barium carbonate at following ratio of components, wt %: pig 3.0-70.0; recycled material 2.0-65.0; broken pieces 0.5-30.0; ferroalloys 1.0-10.0, but limestone, coke and barium carbonate and strontium carbonate or barium carbonate, wt % from weight of charge metal part: limestone 1.5-6.0; coke 10-15.0; barium carbonate and strontium carbonate or barium carbonate 0.01-5.0.
EFFECT: increasing of cast iron casting characteristics and performance attributes of ingots made from it.
2 dwg, 2 ex
Title | Year | Author | Number |
---|---|---|---|
MODIFICATION AND REFINING COMPOUND FOR IRON-CARBON AND NON-FERROUS ALLOYS (VERSIONS) | 2012 |
|
RU2502808C1 |
METALLIC BURDEN FOR PIG IRON SMELTING IN CUPOLA | 2000 |
|
RU2172781C1 |
METHOD OF PREPARING COKE CUPOLA FOR OPERATION | 0 |
|
SU1668835A1 |
ADDITION TO BURDEN OF SHAFT IRON-MELTING FURNACE | 1994 |
|
RU2092568C1 |
CUPOLA HEAT ON HARD COAL | 2009 |
|
RU2407804C2 |
MIXTURE FOR MODIFICATION AND REFINING OF STEEL AND CAST IRON | 2015 |
|
RU2588932C1 |
ALLOY FOR STEEL DE-OXIDATION, REFINING, MODIFYING AND MICRO-ALLOYING (VERSIONS) | 2010 |
|
RU2434966C2 |
METHOD OF STARTING A COKE-FIRED CUPOLA | 0 |
|
SU1537995A1 |
CAST IRON FOR MANUFACTURING CASTING EQUIPMENT (MOLDS) | 2022 |
|
RU2786056C1 |
METHOD FOR PRODUCTION OF CAST IRON AND STEEL UTILIZING BLAST-FURNACE AND STEEL-SMELTING EQUIPMENT ON METALLURGICAL ENTERPRISE | 1998 |
|
RU2137844C1 |
Authors
Dates
2009-01-10—Published
2007-02-19—Filed