FIELD: chemistry, electrochemistry.
SUBSTANCE: invention refers to electrochemistry, particularly to electroplating and can be used in mechanical engineering to ensure corrosion prevention of fabricated metals. Solution contains, wt %: ZnSO4·7H2O 15.0-25.0; Na2SO4·10H2O 10.0-11.0; bone glue 0.20-0.25; dry potato beetle tincture (dry weight equivalent) 0.5-1.0; water the rest.
EFFECT: higher zinc plating brightness and improved current scattering power of solution.
2 tbl, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE OF BRIGHT ZINC PLATING | 2007 |
|
RU2343232C1 |
SHINNING ZINC-PLATING ELECTROLYTE | 1994 |
|
RU2063481C1 |
ELECTROLYTE FOR ELECTRODEPOSITION OF LUSTROUS ZINC COATINGS | 2024 |
|
RU2820435C1 |
SHINE ZINC PLATING ELECTROLYTE | 0 |
|
SU712464A1 |
SHINE ZINC PLATING ELECTROLYTE | 0 |
|
SU711180A1 |
ELECTROLYTE FOR BRIGHT ZINC PLATING | 0 |
|
SU1638214A1 |
BRIGHT ZINC PLATING ELECTROLYTE | 2001 |
|
RU2206641C1 |
METHOD FOR ZINC ELECTRODEPOSITION | 2001 |
|
RU2211887C2 |
ELECTROLYTE AND METHOD OF DECORATIVE NICKELIZING | 1995 |
|
RU2095491C1 |
ZINC-PLATING ELECTROLYTE | 0 |
|
SU665025A1 |
Authors
Dates
2009-03-27—Published
2007-11-19—Filed