FIELD: technological processes.
SUBSTANCE: diameter of hole in plate is set as not more than rod diameter by 0.20 mm. Prior to passage of the main current pulse, heating pulse is passed with current value of 0.6-0.7 from main pulse current and duration of 0.6-0.8 s. Value of main pulse current is selected in the range of (1.2-1.3)I0, where I0 is value of current pulse during welding of packet from two sheets with total thickness equal to plate thickness.
EFFECT: reliable fixation of parts from composite materials.
8 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR RESISTANCE SPOT WELDING OF PIN WITH PLATE FROM TITANIUM ALLOYS | 2007 |
|
RU2352440C2 |
METHOD OF CONTACT SPOT WELDING OF RIVET WITH PLATE OF TITANIUM ALLOYS | 2006 |
|
RU2333085C2 |
0 |
|
SU1669666A1 | |
METHOD FOR WELDING OF THE SPACING GRATES OF THE FUEL ELEMENTS OF NUCLEAR REACTORS | 2003 |
|
RU2262755C2 |
METHOD OF RESISTANCE SPOT WELDING OF WORKPIECES DIFFERING IN THICKNESS | 0 |
|
SU1722744A1 |
METHOD FOR CONTACT SPOT WELDING | 2000 |
|
RU2183152C2 |
METHOD OF MONITORING RESISTANCE SPOT WELDING PROCESS | 0 |
|
SU1715532A1 |
METHOD OF RESISTANCE SPOT WELDING | 0 |
|
SU1018825A1 |
METHOD OF RESISTANCE SPOT WELDING | 0 |
|
SU1031685A1 |
METHOD FOR CONTACT SPOT WELDING | 2002 |
|
RU2225780C2 |
Authors
Dates
2009-04-20—Published
2007-07-19—Filed