FIELD: metallurgy.
SUBSTANCE: invention can be used for processing of chrome ore, concentrates and aluminium-bearing wastes of non-ferrous metallurgy. In the method in the capacity of aluminium-bearing material it is used preprepared aluminium-bearing wastes from manufacturing of secondary aluminium in amount 0.6-1.1 wt % per 1 wt % of content Cr2O3 in chrome-ore concentrate. Isolation of received in furnace melt is implemented with blending during 10-15 minutes, after which it is preliminary pumped out in slag pan 70-90% of dross major part from the total dross mass, then it is pumped out part of the rest slag into metallic reservoir, isolated during 3-5 minutes and discharged the rest part and metal to the same metallic reservoir.
EFFECT: invention provides developing of the new technology of chrome-bearing alloy, providing substitution of expensive reductant by significantly cheaper aluminium-bearing wastes from the aluminium production and increasing of extraction ratio of chrome into the metal.
1 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR ALUMINOTHERMIC OBTAINMENT OF FERROALLOYS | 2013 |
|
RU2549820C1 |
CHARGE FOR OBTAINING HIGH-CARBON FERROCHROME | 2008 |
|
RU2403305C2 |
PROCEDURE FOR PRODUCTION OF LOW CARBON FERROCHROMIUM | 2009 |
|
RU2424342C2 |
METHOD OF ALUMINO-THERMIC PRODUCTION OF LOW-CARBON FERRO-CHROMIUM | 2005 |
|
RU2291217C2 |
METHOD OF PRODUCTION OF LOW-CARBON FERROCHROME IN ELECTRIC FURNACE | 2013 |
|
RU2553118C1 |
CHARGE AND ELECTRIC FURNACE ALUMINOTHERMIC METHOD FOR PRODUCING LOW-CARBON FERROCHROME WITH ITS USE | 2021 |
|
RU2761839C1 |
METHOD OF MAKING CHROMIUM-CONTAINING STEEL | 2002 |
|
RU2222608C1 |
FLUXED CHROME-ORE AGGLOMERATE | 1997 |
|
RU2114060C1 |
METHOD OF PREPARING LOW-CARBON METALS AND ALLOYS | 2000 |
|
RU2164543C1 |
PROCEDURE FOR METAL-THERMAL METAL AND ALLOY MELTING | 2009 |
|
RU2406767C1 |
Authors
Dates
2009-05-10—Published
2007-05-18—Filed