FIELD: metallurgy.
SUBSTANCE: invention relates to foundry field, particularly to composition of exothermal mixtures for heating of feeders of steel and iron castings. Mixture contains aluminium powder, oxidiser, processing aids and silicocalcium with silicon content not less than 50 wt % and calcium not less than 25 wt %, herewith in the capacity of oxidiser it is used dross at following ingredients correlation, wt %: aluminium powder 4.0 - 7.7, dross 57 - 62, silicocalcium 29 - 35, processing aids - the rest.
EFFECT: while using of the mixtur eit is reduced metal consumption for feeders with keeping of high grade of castings.
2 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
EXOTHERMIC SLAG-FORMING MIXTURE | 2010 |
|
RU2429940C1 |
EXOTHERMAL MIX FOR MAKING LOST HEADS | 0 |
|
SU969449A1 |
EXOTHERMIC MIXTURE FOR HEAT INSULATION OF THE HEAD PART OF THE INGOT DURING CASTING OF STEELS AND ALLOYS | 2022 |
|
RU2773977C1 |
METHOD OF HEATING OPEN HEADS OF CAST BLANKS | 0 |
|
SU1560388A1 |
EXOTHERMAL SAND MIXTURE FOR HEATING THE TOP DISCARD | 0 |
|
SU608609A1 |
COMPLEX EXOTHERMAL MIXTURE | 2008 |
|
RU2376101C1 |
EXOTHERMAL MIXTURE FOR HEATING OF HEADS OF STEEL AND IRON CASTINGS | 2008 |
|
RU2369461C1 |
EXOTHERMIC MIXTURE FOR HEATING COPPER AND ALUMINIUM ALLOY CASTING HEADS | 0 |
|
SU814563A1 |
EZOTHERMAL MIXTURE FOR HEATING HEADS OF STEEL CASTINGS | 0 |
|
SU1581469A1 |
EXOTHERMIC MIXTURE FOR HEATING CASTING HEADS | 0 |
|
SU804200A1 |
Authors
Dates
2009-05-27—Published
2007-10-25—Filed