FIELD: explosives.
SUBSTANCE: method to produce porous powder for sporting and fowling cartridges comprises grinding porous powder into powder chips in aqueous medium, preliminary drying, separation and final drying. Note that, after separation, powder chips are processed on mixing by water solution of acetone with concentration of 75 to 80 % by volume for 120 to 150 minutes with subsequent stripping of solvent. Then powder chips are ground in a drum for 90 to 120 minutes in the mix composed of 0.5 % by weight of graphite and 0.8 to 1.0 % by weight of lithium fluoride of the powder chip weight.
EFFECT: improved looseness, receiving powder elements with porous structure with density of 1.0-1.2 g/cm3 and reduced charge weight to 1,0-1,2 g.
4 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING GUN POWDERS INTO FINE-COMBINED POWDERS | 2001 |
|
RU2212394C2 |
METHOD OF PRODUCTION OF THE FINE-GRAIN COMBINED POWDERS | 2004 |
|
RU2285685C2 |
METHOD FOR PRODUCTION OF POROUS POWDER TO SMALL ARMS | 2005 |
|
RU2284980C1 |
POROUS PYROXYLIN POWDER FOR PROPELLANT CHARGES TO CARTRIDGES OF SMALL ARMS OF CIVIL PURPOSE | 2023 |
|
RU2820891C1 |
METHOD FOR PRODUCTION OF POROUS PYROXYLIN GUN POWDER FOR CARTRIDGES FOR SHOOTING WEAPON | 1999 |
|
RU2165402C2 |
TECHNOLOGY PROCESSING PYROXYLIN POWDER TO FINE-WEB POWDERS FOR SMALL ARMS | 2001 |
|
RU2202524C2 |
DIBASIC PYROXYLIN POWDER PREPARATION METHOD | 2002 |
|
RU2242449C2 |
METHOD FOR PRODUCTION OF THIN-ARCHED GUNPOWDER FOR SMALL ARMS CARTRIDGES | 2007 |
|
RU2369587C2 |
SPHERICAL POWDER FOR SPORTING FOWLING PIECE CARTRIDGE CARBINE (7,62×33) | 2010 |
|
RU2451657C2 |
PYROXYLIN PELLET POWDER FOR 5.6 MM SPORT HUNTING CARTRIDGE OF CIRCULAR IGNITION | 2014 |
|
RU2581375C1 |
Authors
Dates
2009-09-20—Published
2007-03-22—Filed