FIELD: metallurgy.
SUBSTANCE: cast-iron products are subject to thermal cycling with heating up to 900-950°C, with isolation during 0.5-1 h and following cooling in boiling water, herewith number of cycles is installed up to three.
EFFECT: reduction of coefficient of linear expansion of cast-iron product.
1 tbl, 1 dwg, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF THERMO-CYCLIC PROCESSING OF IRON | 2008 |
|
RU2370548C1 |
METHOD OF PERIODICALLY HEAT TREATMENT CAST IRON | 2006 |
|
RU2322515C2 |
METHOD OF THERMOCYCLIC TREATMENT OF WHITE CAST IRON | 0 |
|
SU863675A1 |
PROCEDURE FOR THERMAL TREATMENT OF HIGH PURITY IRON | 2009 |
|
RU2418865C1 |
METHOD OF HEAT TREATMENT OF UNALLOYED WHITE CAST IRON CASTINGS | 1999 |
|
RU2152443C1 |
METHOD FOR TEMPERATURE CYCLING OF MULTIPHASE STRAINED IRON-BASED ALLOYS | 2003 |
|
RU2241768C1 |
METHOD OF THERMAL TREATMENT OF LARGE SIZE SLABS OUT OF GRAY PEARLITIC IRON | 2002 |
|
RU2230799C2 |
METHOD FOR PERIODIC HEAT TREATMENT OF CAST IRON | 2006 |
|
RU2322516C2 |
METHOD OF RAPID CEMENTATION OF STEEL DETAILS | 2007 |
|
RU2355816C2 |
METHOD OF TREATMENT OF HIGH-CARBON ALLOYS | 0 |
|
SU1759905A1 |
Authors
Dates
2009-09-27—Published
2008-07-21—Filed