FIELD: chemistry.
SUBSTANCE: composition contains at least one high-molecular polyethylene and at least one low-molecular polyethylene component. The high-molecular polyethylene component of the composition has molecular weight distribution of approximately 6 to 9, content of short-chain branches less than approximately 2 branches per 1000 carbon atoms of the main chain and Mz - approximately 1100000 or greater. The ratio of weight-average molecular weight of the high-molecular polyethylene component to the weight-average molecular weight of the low-molecular polyethylene component is less than 20. The disclosed composition has density greater than 0.94 g/cm3, resistance to cracking under the influence of the surrounding medium greater than 600 hours and percentage swelling greater than 70%.
EFFECT: improved mechanical strength characteristics, suitable for blow moulding.
22 cl, 1 tbl, 16 ex
Title | Year | Author | Number |
---|---|---|---|
HIGH-STRENGTH BIMODAL POLYETHYLENE COMPOSITIONS | 2005 |
|
RU2382800C2 |
POLYETHYLENE COMPOSITIONS | 2009 |
|
RU2493182C2 |
POLYOLEFIN COMPOSITIONS, ARTICLES MADE THEREFROM AND PREPARATION METHODS THEREOF | 2007 |
|
RU2444546C2 |
POLYMERIC POLYETHYLENE COMPOSITIONS AND TUBES MADE FROM SAID POLYMODAL POLYETHYLENE COMPOSITION | 2006 |
|
RU2430123C2 |
POLYETHYLENE RESIN FOR PIPE FITTING | 2005 |
|
RU2375392C2 |
POLYMER COMPOSITIONS AND PROCESS OF TUBE PRODUCTION | 2003 |
|
RU2326904C2 |
COMPOSITION OF EXTRUSION COATING | 2010 |
|
RU2548017C2 |
SUSPENSION POLYMERISATION METHOD | 2008 |
|
RU2469048C2 |
SUSPENSION POLYMERISATION METHOD | 2008 |
|
RU2476448C2 |
POLYMERIC COMPOSITION FOR BLOW MOULDING | 2013 |
|
RU2640594C2 |
Authors
Dates
2009-12-10—Published
2006-06-02—Filed