FIELD: chemistry.
SUBSTANCE: described is a method of processing polytetrafluoroethylene wastes through continuous pyrolysis in the presence of water vapour at high temperature, distinguished by that pyrolysis is carried out in two successive steps, where pyrolysis temperature at the first step is 600-750°C, and 500-600°C at the second step. Temperature at the first step is higher than temperature at the second step.
EFFECT: owing to decomposition in two steps, the method enables simultaneous production of fluoro-monomers and fine-dispersed polytetrafluoroethylene.
2 cl, 4 ex, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING POLYTETRAFLUOROETHYLENE | 2014 |
|
RU2559891C1 |
METHOD OF PROCESSING POLYTETRAFLUOROETHYLENE | 2014 |
|
RU2561111C1 |
METHOD OF OBTAINING FINE-DISPERSED POLYTETRAFLUORETHYLENE | 2006 |
|
RU2326129C1 |
METHOD OF RECYCLING FLUOROPLASTS AND MATERIALS, CONTAINING THEM, WITH OBTAINING ULTRADISPERSE FLUROPLAST AND PERFLUOROPARAFFINS | 2011 |
|
RU2528054C2 |
METHOD FOR PROCESSING POLYTETRAFLUORETHELEN | 0 |
|
SU1775419A1 |
METHOD OF OBTAINING TETRAFLUOROETHYLENE | 2007 |
|
RU2339607C1 |
COMPOSITION OF AT LEAST ONE VINYLIDENE CHLORIDE COPOLYMER | 2008 |
|
RU2476464C2 |
FLUORINATED ELASTOMER LATEX, METHOD OF PRODUCING SAID LATEX, FLOURINATED ELASTOMER AND PRODUCT MOULDED FROM FLUORORUBBER | 2005 |
|
RU2398796C2 |
EQUIPMENT FOR POLYTETRAFLUOROETHYLENE PROCESSING | 0 |
|
SU1763210A1 |
FLUOROPOLYMER LATEX, METHOD OF PRODUCING SAID FLUOROPOLYMER LATEX AND FLUOROPOLYMER | 2005 |
|
RU2376332C2 |
Authors
Dates
2010-04-27—Published
2008-07-14—Filed