FIELD: metallurgy.
SUBSTANCE: invention is intended for protection of steel constructions and facilities against atmosphere corrosion. Inhibitor contains the following, wt %: carboxymethyl cellulose 0.15-0.5; bentonitic clay 0.5-1.0; water - the rest. In the method, as water-soluble polymer, there used is swollen concentrated water solution of carboxymethyl cellulose with degree of polymerisation of 700-900 with content of polymer of 1.5-5.0 wt %, which is mixed with equal quantity of concentrated swollen water solution of bentonitic clay with clay content of 5-10 wt %; then the obtained mass is mixed till homogeneous composition is obtained, and immediately before it is used, there added is design amount of water till the above specified inhibitor is obtained, an the obtained compound is mixed till it is homogeneous.
EFFECT: application of popular cheap polymer and other cheap non-toxic components, simplifying the method, possibility of obtaining the inhibitor at working station.
2 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
INHIBITOR OF STEEL CORROSION AND PROCEDURE FOR ITS PRODUCTION | 2009 |
|
RU2418100C1 |
INHIBITOR OF STEEL CORROSION AND PROCEDURE FOR ITS PRODUCTION | 2010 |
|
RU2418101C1 |
INHIBITOR OF STEEL CORROSION AND PROCEDURE FOR ITS PRODUCTION | 2010 |
|
RU2418102C1 |
STEEL CORROSION INHIBITOR AND METHOD OF ITS RECEIVING | 2007 |
|
RU2353709C2 |
METHOD OF PRODUCING STEEL CORROSION INHIBITOR | 2010 |
|
RU2447199C2 |
METHOD OF PURIFYING SOLID SURFACE AND DETERGENT INTENDED FOR APPLICATION IN METHOD | 2013 |
|
RU2540607C2 |
METHOD OF APPLYING STEEL CORROSION INHIBITOR | 2010 |
|
RU2446896C2 |
METHOD OF OBTAINING COMPOSITION FOR CLEANING AND DISINFECTION OF WATER | 2006 |
|
RU2331470C2 |
METHOD OF PRODUCING POLYMER-MINERAL COMPOSITE | 0 |
|
SU1707052A1 |
ANTICORROSION NANOGEL | 2018 |
|
RU2693250C1 |
Authors
Dates
2010-04-27—Published
2009-01-22—Filed