FIELD: metallurgy.
SUBSTANCE: composition contains, wt %: poly-acryl-amide-gel 0.01-0.02, modified bentonite with contents of montmoryllonite 80 % and over 0.1-0.5 and water - the rest. The procedure for production of inhibitor consists in introducing solution of water suspension of modified bentonite of concentration 2-20 wt % into concentrated water solution of poly-acryl-gel of 0.6-2.5 concentration at operating mixer and at rate of supply not more, than 2 l/min. Calculated amount of water is added into produced mass and is mixed during 3-5 min. If necessary, in field conditions water can be added directly before inhibitor usage. Insignificant concentrations of general access non-toxic components are present in the composition. The finished product is referred to low-hazard bio-de-composed substances.
EFFECT: high protective properties of steel items from corrosion.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
INHIBITOR OF STEEL CORROSION AND PROCEDURE FOR ITS PRODUCTION | 2010 |
|
RU2418101C1 |
INHIBITOR OF STEEL CORROSION AND PROCEDURE FOR ITS PRODUCTION | 2009 |
|
RU2418100C1 |
METHOD OF PRODUCING STEEL CORROSION INHIBITOR | 2010 |
|
RU2447199C2 |
METHOD OF APPLYING STEEL CORROSION INHIBITOR | 2010 |
|
RU2446896C2 |
METHOD OF PURIFYING SOLID SURFACE AND DETERGENT INTENDED FOR APPLICATION IN METHOD | 2013 |
|
RU2540607C2 |
STEEL CORROSION INHIBITOR AND METHOD OF ITS RECEIVING | 2007 |
|
RU2353709C2 |
STEEL CORROSION INHIBITOR AND METHOD FOR OBTAINING THEREOF | 2009 |
|
RU2387740C1 |
INJECTION BENTONITE COMPOSITION FOR WATERPROOFING AND STRENGTHENING OF NATURAL SOIL | 2020 |
|
RU2746327C1 |
METHOD FOR OBTAINING ORGANO-MODIFIED CLAY POWDER FOR PRODUCTION OF PAINT AND VARNISH MATERIALS | 2023 |
|
RU2805707C1 |
SALT-RESISTANT BENTONITE COMPOSITION FOR PREPARING WATER-BASED DRILLING FLUIDS | 2023 |
|
RU2816922C1 |
Authors
Dates
2011-05-10—Published
2010-03-30—Filed