FIELD: construction.
SUBSTANCE: preparation of ceramic slurry is done by means of staged wet grinding mass, including clayey component, thinning agents and fusing agents, at moisture content of 16-20%. Mixture of initial components is previously exposed to thermal activation by means of baking at the temperature of 900-1200°C with further cooling at the following ratio of components, wt %: clayey component - 25-65; thinning agents - 15-50; thinning agents - 0-40. Additionally stabilised chamotte filler may be introduced in amount of up to 50% of weight of the whole dispersed phase.
EFFECT: reduced moisture of cast slurry, increased density of foundry, reduced shrinkage.
2 cl, 1 ex, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING CERAMIC OBJECTS | 2009 |
|
RU2391309C1 |
METHOD OF MAKING ALUMINOSILICATE REFRACTORY ARTICLES | 2009 |
|
RU2408557C1 |
METHOD FOR MAKING WALL CERAMIC ARTICLES (VARIANTS) | 2005 |
|
RU2277520C1 |
CERAMIC CHARGE FOR MANUFACTURE OF PORCELAIN PRODUCTS | 2023 |
|
RU2805702C1 |
METHOD OF MANUFACTURE OF WALL CERAMIC ARTICLES WITH THE USE OF GROUND CRYSTALLIZED GLASS, CHARGE FOR MANUFACTURE OF WALL CERAMIC ARTICLES AND FILLER FOR WALL CERAMIC ARTICLES | 2007 |
|
RU2318771C1 |
METHOD OF MANUFACTURE OF WALL CERAMIC ARTICLES | 2004 |
|
RU2266267C1 |
METHOD OF MANUFACTURE OF WALL CERAMIC ARTICLES, RAW CHARGE FOR MANUFACTURE OF WALL CERAMIC ARTICLES AND FILLER FOR WALL CERAMIC ARTICLES | 2007 |
|
RU2318772C1 |
METHOD OF MAKING CERAMIC WALL PRODUCTS, ROUGH MIXTURE FOR MAKING CERAMIC WALL PRODUCTS, AND FILLER FOR CERAMIC WALL PRODUCTS | 2007 |
|
RU2324668C1 |
METHOD OF MANUFACTURE OF WALL CERAMICS USING SEDIMENTARY HIGH-SILICA ROCKS, STOCK FOR WALL CERAMICS, AND AGGREGATE FOR WALL CERAMICS | 2007 |
|
RU2327666C1 |
METHOD OF MAKING CERAMIC WALL PRODUCTS, ROUGH MIXTURE FOR MAKING CERAMIC WALL PRODUCTS AND FILLER FOR CERAMIC WALL PRODUCTS | 2007 |
|
RU2324669C1 |
Authors
Dates
2010-06-20—Published
2009-04-02—Filed