FIELD: construction.
SUBSTANCE: building mortar, containing dry mix that only requires dilution with water and including the following components, wt %: portland cement 15.0-30.0, quartz sand with grain from 0.1 to 0.5 mm 50.0-70.0, lime flour with grain 0.1-0.5 mm 3.0-10.0, quartz sand with grain up to 0.3 mm 3.0-10.0, modified ether of cellulose 0.05-0.5, hydrophobic reagent - mixture of sodium oleate and calcium stearate 0.05-0.5, pigment 1.0-5.0, flaky silicate of nanometric dimensions 0.05-1.0.
EFFECT: improved resistance to action of migrating salt solutions and salt deposits.
3 cl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
ADHESIVE MORTAR | 2009 |
|
RU2403218C2 |
SANITIZING PLASTER DRY MORTAR FOR BRICKWORK | 2016 |
|
RU2681133C2 |
FINE-GRAINED CONCRETE MIXTURE AND PREPARATION METHOD THEREOF | 2012 |
|
RU2494061C1 |
DRY PACK MORTAR | 2004 |
|
RU2262493C1 |
PRODUCTION OF NANOCEMENT AND NANOCEMENT | 2013 |
|
RU2544355C2 |
DRY PACK MORTAR | 2004 |
|
RU2262494C1 |
ADDITIVE FOR MODIFICATION OF GYPSUM BINDERS, CONSTRUCTION MORTARS AND CONCRETES ON THEIR BASIS | 2014 |
|
RU2572432C1 |
COMPOSITION OF REDISPERSIBLE POLYMER POWDER | 2009 |
|
RU2506285C2 |
DRY PACK MORTAR | 2004 |
|
RU2262495C1 |
APPLICATION OF VINYL CHLORIDE AND ETHYLENE COPOLYMERS FOR HYDROPHOBISATION OF CONSTRUCTION MASSES | 2005 |
|
RU2368583C2 |
Authors
Dates
2011-01-20—Published
2009-01-11—Filed