FIELD: chemistry.
SUBSTANCE: present invention relates to hardeners for unsaturated polyester resins, as well as some other compounds containing double bonds. The hardener is a composition which contains 100 pts. wt benzoyl peroxide, 40-177 pts. wt phthalic ester, 0.6-1.3 pts. wt polyoxyalkylated alkylphenols, 13-97 pts. wt polyoxyalkylated di- or triatomic alcohols with average molecular weight 1000-6000, 1.6-6.0 pts. wt mixture of sodium salts of alkylarylsulphonic acid and 33-43 pts. wt water.
EFFECT: obtaining stable, non-flaking paste with wide range of benzoyl peroxide content.
5 cl, 7 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
FROST-RESISTANT SEALING COMPOUND | 2011 |
|
RU2469062C1 |
METHOD OF PRODUCTION OF COMPOUND MATERIAL FOR POLYURETHANE COAT | 1998 |
|
RU2151160C1 |
METHOD OF PREPARING POLYMER SPORTS COATING | 2008 |
|
RU2393187C2 |
URETHANE PUTTY | 2010 |
|
RU2451703C1 |
COLD HARDENING POLYMERIC COMPOSITION | 2002 |
|
RU2220991C1 |
COATING COMPOSITION | 2010 |
|
RU2448137C1 |
METHOD OF PREPARING POLYMER SPORTS COATING | 2008 |
|
RU2391372C2 |
METHOD OF PREPARING POLYMER SPORTS COATING | 2008 |
|
RU2391371C2 |
COATING COMPOSITION | 2010 |
|
RU2447110C1 |
METHOD OF PREPARING POLYMER SPORTS COATING | 2008 |
|
RU2391373C2 |
Authors
Dates
2011-01-27—Published
2009-06-02—Filed