FIELD: chemistry.
SUBSTANCE: method involves steps for grinding cellulose ether and a cationic surfactant in a mill and, optionally, drying the mixture. Cellulose ether contains water in amount of 20-90% of total weight of the cellulose ether and water. The cationic surfactant is present in amount of 0.001-2% of the total weight of the mixture. The cationic surfactant is a quaternary ammonium compound. Drying is carried out while grinding, before the grinding step or after the grinding step. The method enables to obtain a product with low dust explosion hazard.
EFFECT: obtained cellulose ether is used in cement, gypsum and coating compositions as a thickener and as binder in paints and pharmaceutical preparations.
7 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
SIZING COMPOSITION | 2000 |
|
RU2211274C2 |
METHOD OF PREPARING SPRAY-DRIED FREELY FLOWING CLOTH-SOFTENING COMPOSITION | 1992 |
|
RU2119000C1 |
DISPERSION | 2004 |
|
RU2309213C2 |
COMPOSITION | 2005 |
|
RU2347030C1 |
HOUSEHOLD CHEMICAL COMPOSITIONS | 2017 |
|
RU2736076C2 |
COMPOSITION IN THE FORM OF FLOWING SPRAY-DRIED POWDER FOR SOFTENING FABRIC AND METHOD OF SOFTENING FABRICS | 1992 |
|
RU2123078C1 |
DETERGENT COMPOSITION OR ITS COMPONENT | 2004 |
|
RU2336300C2 |
DETERGENT SOLUTION WITH DISINFECTING PROPERTIES | 2003 |
|
RU2253669C1 |
HAIR TREATMENT COMPOSITIONS | 2008 |
|
RU2487700C2 |
METHOD OF APPLYING COMPOSITION CONTAINING CATIONIC TRIVALENT METAL AND LOOSENER AND SHEET OF LOOSE CELLULOSE MADE THEREFROM | 2010 |
|
RU2610240C2 |
Authors
Dates
2011-04-10—Published
2006-05-09—Filed