FIELD: textile, paper.
SUBSTANCE: ground paper contains a certain amount of cellulose fibres and a gluing substance, besides, ground paper has a coefficient of hygro-expansion from 0.6 to 1.5%, inner link of Scott in cross direction not more than 130 J/m2 and/or inner link of Scott in longitudinal direction of not more than 130 J/m2.
EFFECT: increased stability of dimensions and strength of ground paper surface.
28 cl, 28 dwg, 12 tbl, 5 ex
| Title | Year | Author | Number |
|---|---|---|---|
| PAPER BASES WITH INCREASED SIZING OF SURFACE AND LOW LINEN SIZING WITH HIGH DIMENSIONAL STABILITY | 2007 |
|
RU2449070C1 |
| REGISTRATION SHEET WITH IMPROVED PRINTING QUALITY AT LOW LEVELS OF ADDITIVES | 2009 |
|
RU2517511C2 |
| RECORDING SHEET WITH IMPROVED PRINTING QUALITY AT LOW LEVELS OF ADDITIVES | 2014 |
|
RU2648328C2 |
| COMPOSITION AND SHEET FOR RECORDS WITH IMPROVED OPTICAL CHARACTERISTICS | 2009 |
|
RU2507335C2 |
| COMPOSITION CONTAINING EXPANDABLE MICROSPHERES AND IONIC COMPOUND, AND USE AND PRODUCTION METHODS THEREOF | 2006 |
|
RU2425068C2 |
| PAPER OR CARDBOARD SUBSTRATE COMPRISING CELLULOSIC FIBRES AND EXPANDABLE MICROSPHERES, AND PACKAGING CONTAINER COMPRISING THIS SUBSTRATE | 2006 |
|
RU2506363C2 |
| IMPROVED SURFACE SIZING OF PAPER | 2009 |
|
RU2521636C2 |
| SHEET FOR PRINTING WITH IMPROVED DRYING TIME OF IMAGE | 2011 |
|
RU2517559C2 |
| SHEET FOR PRINTING WITH IMPROVED TIME OF IMAGE DRYING | 2006 |
|
RU2433050C2 |
| IMPROVED METHOD FOR PRODUCTION OF PAPER AND CARDBOARD PRODUCTION | 2007 |
|
RU2401900C1 |
Authors
Dates
2011-05-20—Published
2007-01-17—Filed