FIELD: metallurgy.
SUBSTANCE: procedure for production of multi-layer coating for cutting tool consists in vacuum-plasma application of three-layer coating. Carbonitride of titanium and chromium is applied as a lower layer at pressure of acetylene of 7.5·10-4 Pa and temperature 600°C in a chamber of installation. Same carbonitride alloyed with silicon is applied as an intermediate layer at pressure of acetylene of 7.5·10-4 Pa and temperature 550°C in the chamber of the installation. Carbonitride of titanium and silicon is applied as an upper layer at pressure of acetylene of 4.3·10-3 Pa and temperature 500°C in the chamber of the installation.
EFFECT: increased functionality of tool and upgraded quality of treatment.
2 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414540C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414536C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414541C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414535C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414537C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414542C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2430987C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424361C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424353C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2428508C1 |
Authors
Dates
2011-07-10—Published
2010-04-20—Filed