FIELD: metallurgy.
SUBSTANCE: procedure for production of multi-layer coating for cutting tool consists in vacuum-plasma application of three-layer coating. Carbonitride of titanium and aluminium is applied as a lower layer at pressure of acetylene in the chamber of the installation 7.5·10-4 Pa and temperature 600°C. The same carbonitride alloyed with silicon is applied as an intermediate layer at pressure of acetylene in the chamber of the installation 7.5·10-4 Pa and temperature 550°C. As an upper layer there is applied carbonitride of titanium and silicon at pressure of acetylene in the chamber of the installation 4.3·10-3 Pa and temperature 500°C.
EFFECT: increased functionality of cutting tool (CT) and upgraded quality of treatment.
2 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424357C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414540C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414536C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414535C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414537C1 |
PROCEDURE FOR CUTTING TOOL MULTI-LAYER COATING | 2009 |
|
RU2414542C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2424354C1 |
METHOD OF MAKING MULTILAYER COATING FOR CUTTING TOOL | 2011 |
|
RU2461656C1 |
PROCEDURE FOR PRODUCTION OF MULTI-LAYER COATING FOR CUTTING TOOL | 2010 |
|
RU2428512C1 |
METHOD FOR OBTAINING MULTI-LAYERED COATING FOR CUTTING TOOL | 2011 |
|
RU2464341C1 |
Authors
Dates
2011-07-20—Published
2010-04-13—Filed