FIELD: metallurgy.
SUBSTANCE: according to procedure at products of melt teeming part of boron-containing slag is left in bath of furnace. Siliceous reducer and ore-lime part of charge is loaded on part of boron-containing slag left in a bath of the furnace. 10-20 minutes prior to products of melt teeming mixture of material containing boron oxide with siliceous reducer and lime is charged into slag melt under electrodes. Also, material containing boron oxide in terms of B2O3 is introduced at amount of 0.20-0.30% of weight of slag melt.
EFFECT: reduced losses of chromium with slag, improved performance characteristics and production of slag resistant to silicate decomposition.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
REFINED FERROCHROME SMELTING PROCESS | 2002 |
|
RU2222629C2 |
METHOD OF SMELTING CARBON FERROCHROMIUM | 0 |
|
SU623896A1 |
METHOD FOR SMELTNG MASTER ALLOY BASED ON NITRIDE-FORMING METALS | 0 |
|
SU1036761A1 |
METHOD FOR PREPARATION OF CHROMIUM-NICKEL ALLOY | 0 |
|
SU1804490A3 |
METHOD FOR ALUMINOTHERMIC OBTAINMENT OF FERROALLOYS | 2013 |
|
RU2549820C1 |
METHOD OF PRODUCING LOW-CARBON NICKEL-CONTAINING FERROCHROMIUM | 0 |
|
SU1788067A1 |
METHOD OF REFINED FERROCHROME PRODUCTION | 0 |
|
SU727703A1 |
CHARGE AND METHOD FOR ELECTRIC-FURNACE ALUMINOTHERMIC PRODUCTION OF FERROBORON USING IT | 2013 |
|
RU2521930C1 |
METHOD OF PRODUCTION OF LOW-CARBON FERROCHROME IN ELECTRIC FURNACE | 2013 |
|
RU2553118C1 |
METHOD OF PREPARING NICKEL-CONTAINING ADDITION ALLOY | 1996 |
|
RU2095427C1 |
Authors
Dates
2011-07-20—Published
2009-05-25—Filed