FIELD: textile industry.
SUBSTANCE: method involves water intrusion and boiling of samples of leather fabric. During water intrusion the increase in thickness of leather fabric samples is determined by boiling. Leather fabric samples are measured during water intrusion by means of thickness gauge before boiling and after boiling. Thickness increase of samples is calculated in percents. If thickness of samples increases by more than 50%, leather fabric is subject to mechanical treatment, and namely to scouring.
EFFECT: invention allows determining thickness increase of leather fabric in percents at boiling and based on this the water content which is enough to perform scouring.
3 ex, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DETERMINING AMOUNT OF APPLIED LIQUID DURING LEATHER AND FUR PRODUCTION PROCESSES USING SMEARING METHODS | 2010 |
|
RU2428688C1 |
METHOD OF ANALYSIS OF STRUCTURAL CHARACTERISTICS OF DERMA COLLAGEN | 2010 |
|
RU2425367C1 |
METHOD TO IDENTIFY STRUCTURE-TO-STRUCTURE DISTANCES IN COLLAGEN | 2010 |
|
RU2422823C1 |
METHOD OF FELL BEAMING | 0 |
|
SU1182080A1 |
METHOD FOR SHEEPSKIN TREATMENT | 0 |
|
SU1730163A1 |
METHOD FOR TREATING FURRED PELTS WITH A WEAK SKIN TISSUE | 2019 |
|
RU2711431C1 |
METHOD FOR TREATING FURRED PELTS WITH A WEAK SKIN TISSUE | 2019 |
|
RU2711399C1 |
FUR FELL SOAK PROCESS | 2005 |
|
RU2305709C1 |
PROCESS OF DRESSING SHEEPSKIN WITH HAIR SLIPPING | 0 |
|
SU1172943A1 |
COMPOSITION FOR PRESERVING FURSKIN RAW MATERIAL | 0 |
|
SU1089127A1 |
Authors
Dates
2011-08-27—Published
2010-02-25—Filed