FIELD: construction.
SUBSTANCE: method of rolled bitumen-containing material production includes impregnation of a base with a bituminous composition, prepared by melting and dehydration of the mixture of oil road viscous bitumen with oil construction or insulating bitumen, softening temperature of which is at least 70°C. The melt is cured at the temperature of 120-170°C for 4-8 hours. In process of the composition preparation its softening temperature is evaluated, results of which are used to correct the composition of by addition of one of the components, which provides the composition softening temperature corresponding to the range from 50°C to 71°C. At the same time the bituminous composition is characterised by the following ratio of components, wt %: oil road viscous bitumen - 5-88, oil construction or insulation bitumen - 9-80, plasticising oil - 1-28, such as industrial oil or flax polymerised oil. Also a rolled material is proposed.
EFFECT: finished self-adhesive rolled bitumen-containing material is characterised by improved physical and mechanical properties.
11 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING LAYERED ROOFING AND WATERPROOFING MATERIAL | 2000 |
|
RU2189411C2 |
COMPOSITE RUBBER-BITUMINOUS BINDER AND METHOD OF ITS OBTAINING | 2016 |
|
RU2655334C2 |
POLYMERIC ASPHALT MODIFIER | 2007 |
|
RU2346965C1 |
BITUMEN-CONTAINING MATERIAL | 2002 |
|
RU2220171C1 |
POLYMERIC BITUMEN MODIFIER AND BITUMEN-POLYMER BINDER BASED ON IT | 2015 |
|
RU2615523C1 |
MODIFIED BITUMEN | 2011 |
|
RU2461594C1 |
METHOD OF PREPARING BITUMEN-RUBBER BINDER | 2004 |
|
RU2270846C1 |
BITUMEN MIXTURE FOR ROOFING AND WATERPROOFING MATERIALS | 0 |
|
SU1717606A1 |
BITUMEN-CONTAINING MATERIAL | 1995 |
|
RU2075565C1 |
METHOD FOR ROAD PAVEMENT FORMATION AND ROAD PAVEMENT STRUCTURE OBTAINED BY THIS METHOD | 2016 |
|
RU2633844C1 |
Authors
Dates
2011-09-27—Published
2009-04-02—Filed