FIELD: construction.
SUBSTANCE: glass composition contains SiO2, BaO, Li2O, As2O3, Na2O, K2O, MgO, CaO, ZnO, PbO, SrO, ZrO2, at least one component of the following group: Fe2O3, Cr2O3, MnO, NiO, CoO, at the following ratio of components, wt %: SiO2 - 30.0-35.0; BaO - 1.0-2.0; Li2O - 21.0-25.0; As2O3 - 4.0-5.0; Na2O - 1.0-2.0; K2O - 1.0-2.0; MgO -21.0-25.0; CaO - 1.0-2.0; ZnO - 1.0-2.0; PbO - 1.5-10.0; SrO - 1.0-2.0; ZrO2 -1.0-2.0; at least one component of the following group: Fe2O3, Cr2O3, MnO, NiO, CoO - 0.1-2.0.
EFFECT: reduced temperature of glass boiling.
1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| ENAMEL | 2007 | 
 | RU2343123C2 | 
| GLASS | 2006 | 
 | RU2334699C1 | 
| GLASS | 2006 | 
 | RU2335466C1 | 
| ENAMEL | 2006 | 
 | RU2337076C1 | 
| GLASS | 2006 | 
 | RU2327656C1 | 
| BLACK GLASE | 2009 | 
 | RU2413683C1 | 
| GLASS | 2006 | 
 | RU2329960C1 | 
| GLASS | 2006 | 
 | RU2325343C1 | 
| GLAZE | 2006 | 
 | RU2333169C1 | 
| NONFRITTED GLAZE | 2006 | 
 | RU2350584C2 | 
Authors
Dates
2011-10-20—Published
2010-05-04—Filed